Hello
the formula can be mixed. but will be too thick
Pro Polymer Use only 1.0-1.3% level to get a gel. in the mixing process Please mix all items together except
Zinc PCA then add
Pro Polymer Blend or stir until gel is obtained, then add
Zinc PCA little by little into the formula. Blend or stir to combine. reason for separation
Zinc PCA in the last step Because it looks like an electrolyte, which if added in the first step Creating a gel texture will be more difficult.
This formula can be mixed as well, but
Satin Cream Maker must be increased to a minimum level. more than 2.0% due to
Zinc PCA It is electrolyte and
Satin Cream Maker cannot be tolerated. electrolyte as well as
Pro Polymer in the above formula. one way or another Members can add
Pro Polymer 1% to help create a gel texture in this formula (
Pro Polymer 1%,
Satin Cream Maker 1% shared yes)